Residual Stresses and Nanoindentation Testing of Films and Coatings
Softcover Reprint of the Original 1st 2018 ed.
Book Details
Format
Paperback / Softback
ISBN-10
9811340110
ISBN-13
9789811340116
Edition
Softcover Reprint of the Original 1st 2018 ed.
Publisher
Springer Verlag, Singapore
Imprint
Springer Verlag, Singapore
Country of Manufacture
GB
Country of Publication
GB
Publication Date
Jan 30th, 2019
Print length
207 Pages
Product Classification:
NanotechnologyEngineering: Mechanics of solidsMechanics of solidsTesting of materials
Ksh 21,600.00
Werezi Extended Catalogue
0 in stock
Delivery Location
Delivery fee: Select location
Secure
Quality
Fast
This book covers the basic principles and application of nanoindentation technology to determine residual stresses in films and coatings. Subsequently, nanoindentation is used to determine residual stresses in different types of films and coatings, and to describe them in detail.
This book covers the basic principles and application of nanoindentation technology to determine residual stresses in films and coatings. It briefly introduces various detection technologies for measuring residual stresses, while mainly focusing on nanoindentation. Subsequently, nanoindentation is used to determine residual stresses in different types of films and coatings, and to describe them in detail. This book is intended for specialists, engineers and graduate students in mechanical design, manufacturing, maintenance and remanufacturing, and as a guide to the practice of production with social and economic benefits.
Get Residual Stresses and Nanoindentation Testing of Films and Coatings by at the best price and quality guaranteed only at Werezi Africa's largest book ecommerce store. The book was published by Springer Verlag, Singapore and it has pages.