Superalloys : Strengthening Behavior of Precipitating Phases

Book Details

Format Paperback / softback
ISBN-10 0443456313
ISBN-13 9780443456312
Publisher Elsevier - Health Sciences Division
Imprint Elsevier - Health Sciences Division
Country of Manufacture GB
Country of Publication GB
Publication Date Sep 9th, 2026
Print length 400 Pages
Weight 450 grams
KSh 32,600.00
Temporarily out of stock, due soon 0 in stock

Delivery Location

Delivery fee: Select location

Secure
Quality
Fast
Superalloys: Strengthening Behavior of Precipitating Phases covers the strengthening mechanisms associated with all types of precipitates that form in superalloys, synthesizing a vast body of literature on the strengthening behavior of these phases, with each chapter introducing fundamental metallurgical principles to help readers develop a clear understanding. The book provides an in-depth exploration of the deformation mechanisms of intermetallic phases in superalloys, focusing on the interaction between matrix dislocations and these phases. Chapter 1 provides an overview of superalloys, their classifications, compositions, and the various strengthening phases, also covering the reasons behind the varying strengthening behavior of different precipitates.

Chapter 2 lays the foundation for understanding deformation and strengthening mechanisms in metals and alloys. Chapters 3, 4, and 5 each focus on strengthening behavior and mechanisms of specific precipitates, ?′, ?″, and Ni2(Cr,Mo), respectively. Chapter 6 discusses the strengthening effects of the ? and ? phases, which form at intermediate temperatures and play a crucial role in controlling grain size, enhancing creep, and fatigue resistance. Chapter 7 examines the role of other strengthening agents, including oxides, borides, and carbides that improve high-temperature strength by impeding dislocation motion and grain boundary sliding.

Get Superalloys by Jung Bahadur Singh at the best price and quality guaranteed only at Werezi Africa's largest book ecommerce store. The book was published by Elsevier - Health Sciences Division and it has 400 pages.